EquipmentPublished

Emulsion, coating and stencil quality

The stencil decides what the print can be. Coating technique, drying, exposure testing and the faults that trace back to the darkroom.

  • 12 min read
  • 1,006 words
Emulsion, coating and stencil quality — screen print at a print shop
Equipment12 min readA1printsoft EditorialPhoto: Đồng Phục Hải Triều / Unsplash
On this page7 sections

The short answer

  • Stencil thickness controls edge definition and ink deposit
  • Coat consistently — the same passes every time
  • Emulsion must be bone dry before exposure, in the dark
  • Run an exposure test rather than guessing the time
  • Most press-side faults start in the darkroom

Printers spend a great deal of time adjusting presses to fix problems created in the screen room. The stencil is where edge quality, detail and ink deposit are actually decided, and a screen made carelessly cannot be rescued at the press.

What the stencil does

It controls

  • Which areas of mesh pass ink
  • The sharpness of every edge
  • Ink deposit thickness, through stencil build
  • How much fine detail survives
  • How long the screen lasts on press

The deposit point is the one printers underuse. A thicker stencil holds the ink slightly off the fabric and deposits more, which is why a heavier white benefits from more coating rather than more pressure.

You cannot print sharper than your stencil. Everything after the darkroom is damage limitation.

Choosing emulsion

TypeSuits
DiazoCheap; slower exposure, shorter pot life
Dual cureGeneral purpose; good detail and durability
PhotopolymerFast exposure; convenient
Water resistantPlastisol work
Solvent resistantWater-based and discharge inks
Capillary filmEven thickness; high density work

Resistance is the specification that must match the ink. A water-based or discharge job on emulsion formulated for plastisol will break down mid-run, and that failure is often blamed on exposure — the ink choices are in plastisol or water-based.

Store emulsion cool, dark and sealed, and note the date it was mixed. Old emulsion behaves differently, and a shop chasing an exposure problem is sometimes chasing an emulsion that is past its useful life.

Coating

Consistency above all

  • A clean, degreased and dry screen every time
  • A scoop coater sized to the image, not the frame
  • A fixed number of passes, recorded
  • Print side and squeegee side deliberately, not by feel
  • Steady pressure and speed
  • The same routine from every operator

Recording the coating routine per mesh count is what makes screens repeatable. "Two and one" means nothing unless everyone does the same thing, and variation in coating produces variation in print that gets blamed on the press.

Degreasing is skipped more than any other step and causes pinholes and fish-eyes. New mesh in particular carries residues that prevent emulsion adhering evenly.

Drying

Non-negotiable

  • Dry in complete darkness — any light exposes it
  • Horizontal, print side down
  • Warm, moving air; a dedicated cabinet is best
  • Fully dry before exposure, with no cool damp feel
  • Control humidity where you can
  • Do not rush it with excessive heat

Under-dried emulsion is one of the most common causes of a stencil that will not wash out properly or breaks down on press. Moisture in the coating changes how it exposes, and a screen that felt nearly dry will behave unpredictably.

Humidity makes this seasonal. Drying times that work in summer may be inadequate in a damp workshop in winter, which is worth knowing before blaming a batch of emulsion.

Exposure testing

Exposure time depends on your unit, your emulsion, your coating and your mesh. There is no published number that applies to your shop, and guessing produces persistent low-level problems.

Run a step test

  • Coat and dry a screen exactly as you normally would
  • Expose sections for increasing times
  • Wash out and examine each step
  • Look for the shortest time that fully hardens without losing detail
  • Check fine lines and halftones specifically
  • Record the result per emulsion and mesh count

Retest whenever anything changes — a new emulsion, a new lamp, a different mesh, a different coating routine. LED and metal halide units age differently and both drift, as covered in exposure units.

And check the film before adjusting exposure. Thin or blotchy positives cause symptoms that look exactly like incorrect exposure, which is why film density is the first thing to rule out.

Washout and post-exposure

Finishing the screen

  • Wet both sides gently and let it sit briefly
  • Wash out with moderate pressure, not a jet
  • Rinse until the image is completely clear
  • Dry fully before use
  • Post-expose in daylight or the unit to harden it
  • Block out pinholes and tape the edges

Post-exposure meaningfully extends screen life for a minute's work, and it is the step most often skipped. A hardened stencil resists both aggressive inks and long runs.

Inspect against a light before racking. Pinholes found now cost a dab of blockout; found on press they cost a stopped run and spoiled garments.

Common faults

FaultUsual cause
Image will not wash outOverexposed, or film not dense enough
Stencil breaks down on pressUnderexposed, or under-dried
PinholesDust, or inadequate degreasing
Ragged edgesUneven coating or poor film contact
Fine detail lostOverexposure, or coating too thick
Fish-eyes in the coatingGrease on the mesh
Sawtooth edgesCoarse mesh for the detail required

Notice how many of those have opposite causes. Overexposure and underexposure produce different failures, which is exactly why a step test is worth an hour — it replaces guessing with a number.

Keep the darkroom genuinely dark and genuinely clean. Stray light fogs emulsion slowly enough that nobody connects the two, and dust is responsible for most pinholes — both are environmental problems rather than technique problems, and neither is fixed by adjusting exposure.

Reclaim properly as part of the same discipline. Emulsion residue left in the mesh, or ghost images from a previous job, affect how the next stencil sits and how evenly it coats, so the screen room's output depends on its reclaim as much as on its coating.

Record the settings that work and treat them as a standard rather than a starting point. A screen room with written coating routines, tested exposure times per emulsion and a drying process everyone follows produces consistent screens, and consistent screens are what let a printer stop compensating at the press. The rest of the equipment archive assumes the stencil was made to a recorded process.

Filed underEquipment
Share
Written byA1printsoft Editorial
175 articles

The print production desk at A1Printsoft. Writes the practical side of running a decorating shop: what things cost, how long they take and what to charge, checked against published trade figures.

Keep reading

More on equipment

All Equipment articles

Set up in an afternoon. From what you already do.

Free for 14 days · no card · pick what you make and we preload the methods, products and price tables.